Large-area spatial atomic layer deposition of amorphous oxide semiconductors at atmospheric pressure

Schrijver

Huibert Bijland

Onderwerp Publications
Gepubliceerd op

May 1, 2019

Publication source

Journal of the Society for Information Display

Volume 27, Issue 5, May 2019, Pages 304-312

Authors

Katsouras I., Frijters C., Poodt P., Gelinck G., Kronemeijer A.J.

Abstract

Indium gallium zinc oxide (IGZO) is deposited using plasma-enhanced spatial atomic layer deposition (sALD) on substrates as large as 32 × 35 cm 2 . Excellent uniformity and thickness control leads to high-performing and stable coplanar top-gate self-aligned (SA) thin-film transistors (TFTs). The integration of a sALD-deposited aluminum oxide buffer layer into the TFT stack further improves uniformity and stability. The results demonstrate the viability of atmospheric sALD as a novel deposition technique for the flat-panel display industry.   

Copyright © 2019 Society for Information Display. 

Read the whole article published in the Society for Information Display here. 

Funding text

The authors would like to thank the process engineers of Holst Centre’s GEN1 R&D (TFT) Pilot Line for the fabrication of the TFT backplanes. This work was financed by the Flexlines project within the Interreg V‐programme Flanders‐The Netherlands, a cross‐border cooperation program with financial support from the European Regional Development Fund, and cofinanced by the Province of Noord‐Brabant, The Netherlands.

Paul Poodt
Chief Technology Officer
Learn more about spatial ALD

Are you interested to learn how plasma-enhanced spatial ALD can help your innovation? Schedule a meeting with our team to learn more about our unique spatial ALD technology and state-of-the-art product portfolio.